Effects of Water, Alcohols Impurities in Polyaspartic Flooring Formulation The influence of water and small molecular alcohols on the reaction rate is remarkable A Solvent water content and purity B Powder water content C Dilute solvents for additives such as leveling agent, defoaming agent, etc. Wa... 더보기
➤ 방문 웹사이트
살포 Polyaspartic 날씨 저항 코팅 정립 철수 테스트 문제
가격: Negotiable
MOQ: 200KG
배달 시간: 7 days after getting order
상표: Feiyang Novel Materials
Problem: pull-out test brush is OK, but spraying film failed, only 3-4Mpa, polyaspartic topcoat film delaminate level by level when doing pull-out test. Request Date: Pull-out Testing above 7.5Mpa. Background: 1. metal substrate 2. Polyaspartc topcoat on polyurethane 3. Machine spraying. Problem: pu... 더보기